Reactive Wetting of an Iron-Based Superalloy MSA2020 and 316 Stainless Steel by Molten Zinc Alloy...

by Xingbo Liu, Jing Xu, Mark A Bright, James G Hemrick, Ever J Barbero
Publication Type
Journal
Journal Name
Metallurgical and Materials Transactions A
Publication Date
Page Numbers
1382 to 1391
Volume
39A
Issue
6