Performance of Wrought Superalloys in Extreme Environments

by Bruce A Pint
Publication Type
Conference Paper
Journal Name
The Minerals, Metals & Materials Series
Publication Date
Page Numbers
165 to 178
Volume
9
Conference Name
9th International Symposium on Superalloy 718 and Derivatives
Conference Location
Pittsburgh, Pennsylvania, United States of America
Conference Sponsor
TMS
Conference Date
-

As power generation systems move towards higher efficiency operation above 700 ℃, wrought superalloys are the leading structural alloy candidates, including precipitation strengthened (PS) alloys 740 and 282 for the highest temperatures. To evaluate the performance of these alloys for these applications, a range of 500–5000 h evaluations have been conducted in environments including steam, supercritical CO2 (sCO2) and simulated combustion exhaust with H2O and/or SO2 at 700–800 ℃ and compared to baseline exposures in laboratory air and 1 bar CO2. These alloys primarily rely on the formation of an external Cr-rich oxide layer or scale for environmental protection and the reaction rates in all of these conditions are similar and relatively low. However, compared to a conventional solid solution strengthened alloy, like 625, the mass gains are higher for PS alloys due to the Âé¶¹Ó°Òô oxidation of the γ′ forming additions, Al and Ti. Post-exposure characterization has quantified the reaction products and the depth of Âé¶¹Ó°Òô oxidation is not a concern and does not appear to increase above the baseline behavior in laboratory air. Likewise, there is no indication of Âé¶¹Ó°Òô carburization in the sCO2 environment at 750 ℃/300 bar. The addition of 0.1% SO2 in CO2-10% H2O at 800 ℃ actually suppressed the Âé¶¹Ó°Òô oxidation at 1 bar but SO2 may be a concern when the total pressure is higher.