Oxidation Resistance: One Barrier to Moving Beyond Ni-Base Superalloys...

by Bruce A Pint, James R Distefano, Ian Wright
Publication Type
Journal
Journal Name
Materials Science and Engineering A
Publication Date
Page Numbers
255 to 263
Volume
415
Issue
1-2