Influences of Surface Preparation on Nanoindentation Pop-in in Single Crystal Mo...

by Zhigang Wang, Hongbin Bei, Easo P George, George Pharr
Publication Type
Journal
Journal Name
Scripta Materialia
Publication Date
Page Numbers
469 to 472
Volume
65