Publication

High-Temperature Mechanical Properties and Microstructure of Cast Ni-based Superalloys for Steam Turbine Casing Applications...

by Philip J Maziasz, Neal Evans, P. Jablonski
Publication Type
Conference Paper
Publication Date
Page Numbers
900 to 915
Volume
n/a
Conference Name
6th International Conference on Advanced materials Technology for Fossil Power Plants
Conference Location
Santa Fe, New Mexico, United States of America
Conference Sponsor
EPRI
Conference Date
-

Proceedings from the 6th International Conference, 2011, pp.900-915 ISBN: 9781615037247