Evolution of Microstructure in a Nickel-based Superalloy as a Function of Ageing Time

Publication Type
Journal
Journal Name
Philosophical Magazine Letters
Publication Date
Page Numbers
483 to 490
Volume
91
Issue
7

An experimental investigation, combining synchrotron X-ray powder diffraction, small-angle neutron-scattering, and transmission electron microscopy, has been undertaken to study the microstructure of nanoprecipitates in a nickel-based superalloy. Upon increasing the ageing time during a heat-treatment process, the average size of the precipitates first decreases before changing to a monotonical growth stage. Possible reasons for this observed structural evolution, which is predicted thermodynamically, are suggested.