Effect of Loading History on Stress Corrosion Cracking of 7075-T651 Aluminum Alloy in Saline Aqueous Environment

by Sergiy Kalnaus, Jixi Zhang, Yanyao Jiang, Majid Behrooz
Publication Type
Journal
Journal Name
Metallurgical and Materials Transactions A
Publication Date
Page Numbers
448 to 460
Volume
42
Issue
2